The wear-resistant material delivery pipeline is the blood of industrial production, and ensuring the service life of the pipeline is the premise of safe and efficient production. The wear of straight pipes is usually much less than that of curved pipes. Therefore, the wear of the elbow is mainly considered in pneumatic conveying.
For example, the conveyed material is an abrasive material such as iron powder. If the ordinary steel elbow is used for continuous conveying for 2 hours, the elbow will be worn; if the bending radius of the elbow is too small, the breakage rate of the elbow will increase when transporting brittle materials
If the bending radius is too large, stringing can occur when transporting synthetic materials.
According to long-term experience, the main factors that cause wear due to material impact or friction on the inner wall of the pipe are as follows:
(1) The physical properties of the material to be transported. Including particle size and shape, concentration, hardness, moisture content, breakage rate and adhesion.
(2) Condition of the delivery pipe. Including the material and metal structure composition, hardness, surface treatment, inner diameter, arrangement and shape of the delivery pipe.
(3) Delivery Conditions. Including conveying air speed, material to gas ratio, temperature and flow state, etc.
In actual transportation, the influence of the above factors on wear and tear does not exist alone, but appears comprehensively. Therefore, even for the same material, there are different conveying conditions and different degrees of wear.