Alumina Powder CAS No. 1344-28-1 Used in Wear-Resistant Materials, Polishing Materials, Welding Materials and Ceramic Glaze.

Alumina Powder CAS No. 1344-28-1 Used in Wear-Resistant Materials, Polishing Materials, Welding Materials and Ceramic Glaze.

Application of wear-resistant ceramic lining: it is the wear-resistant material for material conveying equipment or liquid flowing through the pipeline surface in petroleum, mining, steel plant, power plant and other industries. Its main function is to effectively resist the impact of material on the pipe wall when passing, the corrosion of chemical substances and the thermal impact of material passing, reduce the wear of equipment components, thus greatly reducing the low-frequency complex maintenance It is the first choice of wear-resistant, impact resistant and corrosion-resistant materials for industrial use.
Send Inquiry
Product Introduction

Our Alumina grinding media balls, Alumina Grinding Open Hole Balls, alumina grinding media have been sold all over the world and have created a national brand to lay a solid foundation. To be the real winner, starts here! We have been unanimously recognized by users with our enthusiastic service and professional knowledge.

Product introduction

The wear-resistant alumina ceramic lining board is a new type of special corundum ceramics, which is made of Al2O3 as the main raw material, rare metal oxides as the solvent, high temperature sintering at 1650 ° C, and inorganic special binders..It is the ideal material for conveying equipment in power, metallurgy, coal, petroleum, cement, chemical industry etc. Its service life is more than ten times than cast stone and wear resistant alloy cast steel.



Feature

1.Wear resistant alumina ceramic lining square plate has good electrical conductivity, mechanical strength and high temperature resistance, far exceeding the wear resistance of wear-resistant steel and stainless steel.

2.Alumina ceramic tiles has obvious advantages such as high hardness, good wear resistance, strong impact resistance, light weight and good stability.

3.simple installation, low cost, and saving maintenance time.


Specification available

Size

Length (L)

Width

Height

Flat lining

50-150

25-100

6-50

Weldable lining

50-150

30-100

10-50

Trapezoidal lining

50-150

20-100

8-50

NOTE: Dimension can be customized according to customers' requirements.


Chemical composition and physical properties

Series

BM92

BMG95BME95BMZTA

BMZR

Al2O3(%)

92±0.5

95±0.595±0.5≥75

-

ZrO2(%)---≥2194.8±0.5

Bending strength(Mpa)

≥220

≥250≥300≥400

≥800

Compressive strength(Mpa)

≥1050

≥1300≥1600≥2000

-

Fracture toughness

(MPam1/2)

≥3.70

≥3.80≥4.0≥4.5

≥7

Rockwell hardness(HRA)

≥82

≥85≥88≥90

≥88

Wear volume(cm3)

≤0.25

≤0.2≤0.15≤0.05

≤0.02

Bulk density(g/cm3)

≥3.6

≥3.65≥3.7≥4.1

≥5.9


Application

Wear resistant alumina ceramic lining square plate is widely used in hoppers, chutes, ball mills,etc of the steel, cement, mine, chemical industry etc.


Picture

IMG_4379


Our ceramic tiles

 logo


The production process

brick

All our employees will continue to work hard to continuously update the Alumina Powder CAS No. 1344-28-1 Used in Wear-Resistant Materials, Polishing Materials, Welding Materials and Ceramic Glaze. to meet the needs of customers. The company has always adhered to the quality of survival, to the management of efficiency, we take the brand as the guidance. Since our establishment, our company has continuously improved, perfected and upgraded existing equipment, and increased the research and development of new equipment and technology, so that our products always have strong core competitiveness.

Send Inquiry