The wear of the pulverized coal elbow is a very troublesome problem. The wear of the pulverized coal on the pipe wall is very serious under the high-speed movement. In addition, the centrifugal force at the elbow makes the elbow wear extremely serious. The wear resistance has a very limited life just now, which greatly increases the maintenance cost and increases the workload. Today, I will introduce a new anti-wear treatment method for elbows.
The hardness of ordinary wear-resistant steel is only about Mohs level 7, so it is easy to wear under the high-speed scouring of pulverized coal. To solve this problem, we can increase the lubricity or improve the hardness of the pipe wall from two aspects. It is not easy to increase lubricity in this rough production environment, so increasing the hardness of the pipe wall is our better direction. Through the actual production inspection, it can be seen that the anti-wear effect of the elbow protected by the wear-resistant ceramic sheet is more prominent. The hardness of the wear-resistant ceramic sheet is Mohs 9, second only to diamond. The use of paste spot welding process stipulates that the inner wall of the elbow can have a good protection effect, and the actual service life is more than ten times that of the steel pipe, which greatly reduces the maintenance workload and maintenance cost and ensures production to the greatest extent.