Surface cleaning → body repair → grinding operation → paste ceramic → welding → test thickness → self-test
1. Preparatory work: purchasing materials, commissioning equipment, arranging construction personnel, connecting the power supply and air source and other preparatory work.
2, surface cleaning: effectively remove dirt, floating embroidery and other sundry
3. Grinding operation: The Angle grinder is used to treat the sprayed pipe wall, requiring no loose animals such as floating embroidery on the pipe surface. Construction is strictly prohibited in the environment with humidity greater than 85%, so as to ensure the quality of the project meets the excellent standard.
4. Isolation measures: After removing debris, stand in a dry environment to prevent dust pollution.
5, paste ceramic lining plate: according to the proportion of mixed A and B components, evenly mixed paste ceramic, paste wear-resistant ceramic plate, stick 0.4 wipe evenly, there will be no virtual adhesion and process phenomenon, wear-resistant ceramic layer surface is smooth, and the gap between pieces will be less than 0.4mm. The ceramic joint is smooth and smooth.
6. Welding: Put the hardware into the hole of the ceramic lining plate after adhesive, weld a circle with the welding machine, and then paste the ceramic cap on the surface of the hardware.
7. Self-inspection: After pasting wear-resistant ceramic pieces, self-quality inspection is carried out, and unqualified parts are processed again