Wear Resistant Ceramic Lined Pipe with Metal and Adhesive

Wear Resistant Ceramic Lined Pipe with Metal and Adhesive

High temperature ceramic adhesive is called high temperature wear-resistant ceramic adhesive. It refers to a kind of high-function adhesive which is used to copy wear-resistant ceramic sheet or lining plate to the surface of equipment substrate above high temperature (usually greater than 200 ℃) working condition to implement wear-resistant protection on equipment substrate.
Send Inquiry
Product Introduction

Our company mainly deals in Wear Resistant Ceramic Tubes, Microcrystalline Wear Resistant Alumina Liner, Inert ceramic balls, and can also develop and design related products according to customer requirements. Our service is based on tracking service to ensure the interests of customers and we have won the favor of the majority of users relying on excellent quality and service over the years. Our company has always adhered to the concept of developing identification equipment that meets the future needs of customers.

Usage of high temperature ceramic adhesive:

1. Before high temperature ceramic adhesive bonding, polish the surface of bonded parts with 100-120 abrasive cloth, and then remove oil with acetone. If possible.

2. High temperature ceramic glue can dry quickly at room temperature. Generally, 600 grams of glue should be prepared at one time. Please use it up within 30 minutes. It is better to use a container with a large bottom area for loading. Please make preparations before use, how much to use and how much to use now.

3. Accurately weigh the two components of AB in a clean and dry container according to the ratio with a pharmaceutical balance, and operate the ratio according to 1:1.Mix well and set aside. Apply the glue evenly on the treated ceramic piece (the amount of glue should be appropriate).Then carry out lamination according to the requirements of the drawing, and remove the extruded.

 

 

 

 

 

Technical Data

Series BM8080 BM2011 BM8180
Color White

White

(light yellow)

Grey/White
Density(g/cm3) 1.28 1.66~1.70 1.48~1.52
Weight ratio(A:B) 4:1 1:1 4:1
Volume ratio(A:B) 4:1 1:1 4:1

Operation time

(200g mixing, min)

30 30 30
Full curing time(h) 24 24 24

Tensile strength(Mpa)

GB/T6329-1996

65.0 65.0 35.0

Shear strength(Mpa)

GB/T7124-2008

≥10 ≥10 ≥18
Working temperature (℃) -60~150 -60~150 -60~200
Expiration date(years) 2 2 2

 

1

 

Product photo

High Temperature Wear Resistant Ceramic Adhesive3High Temperature Wear Resistant Ceramic Adhesive4

Application

2

 

 

 

 

 

Due to the wide application of our products and our favorable market position, we strive to sell our Wear Resistant Ceramic Lined Pipe with Metal and Adhesive to more countries and bring our high-quality products and services to every corner of the world. We integrate and upgrade the customer relationship management, automated order decomposition, and intelligent warehousing systems. The various products we produce are constantly becoming more humanized in design, facilitating daily life and industry.

Send Inquiry

whatsapp

Phone

E-mail

Inquiry